With over 40 years of experience, our production site in Indiana, USA, is a leading manufacturer of ready-to-install products and components made of tungsten composites and tungsten alloys. From Indianapolis, we supply more than 10,000 customers in the aerospace, defense, medical technology, oil and gas, and mechanical engineering industries.

To ensure the high quality of our products, we cover the entire process chain in-house – from powder mixing to precision machined components, quality control, sales, and customer service.

Our core competencies at Mi-Tech Tungsten Metals:

  • Decades of experience in the development and production of high-quality tungsten alloys and tungsten composites including mill products and precision machined components
  • Compliance with strict quality control procedures throughout the entire manufacturing process
  • State-of-the-art manufacturing processes – from raw material to ready-to-install components
  • Extensive experience in material processing, such as grinding, turning, and milling, to be able to implement technical customer specifications quickly, precisely, and in high quality
USA, Indianapolis

Mi-Tech Tungsten Metals

4701 Massachusetts Ave.46218 Indianapolis
Tel:+1 800 624 1895Fax: +1 317 549 4295
Find us with Google Maps
At a glance
    Materials

    Materials with special properties

    At Mi-Tech Tungsten Metals, we specialize in the powder metallurgical production of tungsten-based alloys and composites such as tungsten heavy alloys (WHA) and tungsten-copper and tungsten-silver composites.

    The advantages of our materials at a glance

    • High-density WHA of 17.0 to 18.5 g/cm3
    • High modulus of elasticity, very good mechanical properties
    • High absorption capacity for X-rays and gamma rays
    • Safe for human health and the environment
    • High wear resistance
    • Good thermal conductivity
    • Good electrical conductivity
    • All our materials at a glance

      Tungsten heavy metal with a density of 17.0 to 18.5 g/cm3

      • ASTM-B-777 Class 1 – 4

      Tungsten-copper with a density of 12.5 to 15.5 g/cm3

      • W55Cu45
      • W68Cu32
      • W70Cu25
      • W78Cu22
      • W80Cu20

      Tungsten-silver with a density of 13.4 to 15.5 g/cm3

      • W50Ag50
      • W65Ag35
      • W74Ag26

      These materials offer a unique combination of density, mechanical strength, and shielding effect.

    Products and applications

    Our products and components are used wherever particularly high demands are placed on the material. They are utilized especially in the defense industry as well as in the manufacture of sports equipment, in die-casting applications, and in machining and tooling processes worldwide.

    Satellites

    Our high-density alloys are used in rotor blades, propellers, inertial systems, and other aerospace applications

    X-ray scan

    Airport package, luggage, and personal X-ray devices contain Mi-Tech tungsten alloys, which can also be found in large-container inspection equipment.

    Chassis

    Our chassis weights made from high-density alloys consume considerably less volume than their lead counterparts. They are designed for balance and lowering the car's center of gravity and are used in the auto racing segment. 

    • slideplansee-aem/components/imageSlide66623713
    • slideplansee-aem/components/imageSlide66623715
    • slideplansee-aem/components/imageSlide66623717
    Certifications

    Our promise of quality and our responsibility

    At Mi-Tech Tungsten Metals, we look after the health and safety of our employees. As a responsible company, we protect the environment and adopt a conscientious approach to raw materials and resources. Our quality management system is certified according to AS9100:D and ISO 9001:2015.

    To the 9100/9001 certificate
    Further information

    Want to find out more about our site in Indianapolis? Visit the company website!